Mostrar el registro sencillo del ítem

dc.contributor.authorRivas Montoya, Ernesto
dc.contributor.authorMartín Lara, María Ángeles 
dc.contributor.authorBlázquez García, Gabriel 
dc.contributor.authorPérez Muñoz, Antonio 
dc.contributor.authorCalero De Hoces, Francisca Mónica 
dc.date.accessioned2020-05-08T09:45:19Z
dc.date.available2020-05-08T09:45:19Z
dc.date.issued2019-05-04
dc.identifier.citationRivas, E.; Martín-Lara, M.Á.; Blázquez, G.; Pérez, A.; Calero, M. Column Leaching Tests to Valorize a Solid Waste from the Decommissioning of Coal-Fired Power Plants. Energies 2019, 12, 1684. [doi:10.3390/en12091684]es_ES
dc.identifier.urihttp://hdl.handle.net/10481/61902
dc.descriptionThe authors are grateful to the Minera de Órgiva, S.L., Granada, Spain for financial support, supply of materials used for experiments and approval of this work for publication. Also, authors would like to thank to Celso Amor for his helpful advice on various technical issues oriented to scale-up.es_ES
dc.description.abstractSolid waste from the decommissioning of coal-fired power plants collected from a power plant in Spain (Puertollano, Ciudad Real) was subjected to acid leaching tests in columns to evaluate the leachability of several valuable and toxic metals (Al, Ca, Fe, K, Mg, Na, Ti, V, Cr, Mn, Ni, and Zn). First, the contaminated waste, delivered by a national company, was chemically characterized. Second, column-leaching tests were conducted using two different acid solutions (nitric and sulfuric acid). The effect of the leaching agent concentration and time of leaching were examined. The results of column leaching tests showed that different concentrations of the acid solutions leached different proportions of Al, Fe, Mg, Mn, Ni, V, and Zn, which were leached by acid solutions from the solid waste sample. In general, use of sulfuric acid at pH 0.5 resulted in better leaching. Next, a comparison between three different configurations (one single stage without recirculation, one single stage with total recirculation of leachate and leaching in two consecutive stages: one with total recirculation of leachate and another one with acid set to a pH value of 0.5 and without recirculation) was performed. At the end of the experiments, all leaching methods resulted in comparable yields for Al (0.36–0.48%), Fe (5.99–6.40%), Mg (4.43–5.11%), Mn (2.71–2.83%), Ni (12.08–12.75%), V (0.08–0.34%), and Zn (23.62–25.28%). However, better results were obtained when two consecutive stages were carried out. Additionally, the effect of forced aeration on leachability was studied. Finally, this investigation showed that hydrometallurgical treatment of contaminated solid by means of acid leaching followed by basic leaching and a water wash between these stages was a potentially feasible method for reducing hazardous levels of the residue.es_ES
dc.description.sponsorshipThis research was funded by MINERA DE ÓRGIVA, S.L.es_ES
dc.language.isoenges_ES
dc.publisherMDPIes_ES
dc.rightsAtribución 3.0 España*
dc.rights.urihttp://creativecommons.org/licenses/by/3.0/es/*
dc.subjectAcid leachinges_ES
dc.subjectCoal-fired power plantses_ES
dc.subjectColumn systemses_ES
dc.subjectMetals es_ES
dc.subjectSulfuric acides_ES
dc.subjectWaste processinges_ES
dc.titleColumn Leaching Tests to Valorize a Solid Waste from the Decommissioning of Coal-Fired Power Plantses_ES
dc.typeinfo:eu-repo/semantics/articlees_ES
dc.rights.accessRightsinfo:eu-repo/semantics/openAccesses_ES
dc.identifier.doi10.3390/en12091684


Ficheros en el ítem

[PDF]

Este ítem aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del ítem

Atribución 3.0 España
Excepto si se señala otra cosa, la licencia del ítem se describe como Atribución 3.0 España